A few pieces I did today in the Raku kiln , and fumed with stannus chloride . Very nice
Welcome to a spot where you will get to experience my ongoing love affair with my life
Showing posts with label fuming. Show all posts
Showing posts with label fuming. Show all posts
Monday, January 5, 2015
Wednesday, November 12, 2014
A new process
I tried a new to me process this past weekend , fuming , where you open the kiln at about 900 degrees f and add some stannus chloride and that creates the fumes , then wait till its cooled . What you see here is the result of my first try
Subscribe to: